EN8 STEEL
A cost-effective steel for general engineering.
EN8 is an unalloyed medium carbon steel known for its high strength, durability, and good resistance to wear and temperature. It is widely used in general-purpose engineering applications where alloy steels are not economically justified. Compared to alloy steels, EN8 offers a more cost-effective solution while still providing dependable mechanical performance.
EN8 steel chemical composition.
| Element | Content (%) |
|---|---|
| Carbon (C) | 0.35 – 0.45 |
| Manganese (Mn) | 0.60 – 1.00 |
| Silicon (Si) | 0.05 – 0.35 |
| Phosphorus (P) | ≤ 0.06 |
| Sulphur (S) | ≤ 0.06 |
Performance for general engineering.
Material Type: Medium Carbon, Unalloyed Steel
Strength: High tensile strength with good toughness
Surface Properties: Excellent surface hardness with moderate wear resistance when flame or induction hardened
Heat Treatment: Can be heat-treated to achieve higher hardness and tensile strength
Machining: Good machinability; weldability is fair (precautions required)
Cost Efficiency: Lower cost than alloy steels with sufficient strength for standard applications
EN8 available in multiple forms.
Bright Bars
EN8D Carbon Steel Bright Bars are available for improved dimensional accuracy and surface finish
Ground Bars
Precision-ground or surface-ground rods supplied as per customer specifications
Cut-to-Size
Bars available in round, square, flat, and hexagonal profiles, cut to required dimensions
EN8 available in the shapes you need.
Kuber Multi Metals is the largest stockiest and supplier of EN8 tool steel in flat, square and round bar. We provide steel in all sizes as your requirements. EN8 die steel is available in flat, square and round shape. Consult our team who will assist you for EN8 steel query.
Strength and hardness.
| Condition | Tensile Strength (MPa) | Yield Strength (MPa) | Hardness (HB) | Elongation (%) |
|---|---|---|---|---|
| As rolled / Normalized | 550 – 660 | ~280 | 152 – 207 | 16 – 22 |
| Quenched & Tempered | 600 – 1000 (varies with tempering) | 400 – 650 | 200 – 300 | 10 – 15 |
Controlled treatment for required performance.
| Process | Temperature Range (°C) | Notes |
|---|---|---|
| Normalizing | 830 – 860 | Air cool |
| Annealing | 680 – 700 | Furnace cool |
| Hardening | 820 – 860 | Oil or water quench |
| Tempering | 550 – 660 | To required hardness/strength |
Built for general engineering.
Strength, hardness and cost-effective performance.
EN8 medium carbon steel is the best and cheapest alloy option for various engineers and automotive applications. Its combination of strength and hardness makes this grade a rather effective wear resistance, with quite good performance without exorbitant costs for alloy steels. It has thermal versatility and is manufactured into different product forms applicable for use in shafts, gears, bolts, and machines, and so suitable for wear during long-term or harsh conditions.